How do I choose the correct joint treatment?

|   Interior

By joint treatment with AQUAPANEL® Joint Adhesive (PU), expansion joints should be at a minimum of 7.5 m intervals, and by joint treatment with AQUAPANEL® Joint Filler & Skim Coating – white, expansion joints should be at a minimum of 15 m intervals. For indoor boards we recommend AQUAPANEL® Joint Adhesive (PU) when using cladding finishes.